PbWO4 crystal for laser energy accumulation and transformation


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The picosecond interband two-photon laser excitation of PbWO4 crystals at a temperature of 10 K leads to electronic excitation energy accumulation, which results in almost 100% induced absorption in the 450–750 nm spectral range. The relaxation time of this induced absorption exceeds 100 min. The electronic excitation energy accumulated in the PbWO4 crystal at T = 10 K excites the intrinsic luminescence with a decay time longer than 45 min. The decay kinetics and the spectra of the intrinsic luminescence of the PbWO4 crystal at a temperature of 10 K were measured under two-photon and single-photon excitation. The luminescence under two-photon and single-photon excitation revealed a difference in the structure of the spectra.

Об авторах

V. Lukanin

Prokhorov General Physics Institute

Email: karasik@lst.gpi.ru
Россия, ul. Vavilova 38, Moscow, 119991

A. Karasik

Prokhorov General Physics Institute

Автор, ответственный за переписку.
Email: karasik@lst.gpi.ru
Россия, ul. Vavilova 38, Moscow, 119991

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).