PbWO4 crystal for laser energy accumulation and transformation
- Авторлар: Lukanin V.I.1, Karasik A.Y.1
-
Мекемелер:
- Prokhorov General Physics Institute
- Шығарылым: Том 121, № 4 (2016)
- Беттер: 503-506
- Бөлім: XVI International Feofilov Symposium
- URL: https://ogarev-online.ru/0030-400X/article/view/165043
- DOI: https://doi.org/10.1134/S0030400X16100143
- ID: 165043
Дәйексөз келтіру
Аннотация
The picosecond interband two-photon laser excitation of PbWO4 crystals at a temperature of 10 K leads to electronic excitation energy accumulation, which results in almost 100% induced absorption in the 450–750 nm spectral range. The relaxation time of this induced absorption exceeds 100 min. The electronic excitation energy accumulated in the PbWO4 crystal at T = 10 K excites the intrinsic luminescence with a decay time longer than 45 min. The decay kinetics and the spectra of the intrinsic luminescence of the PbWO4 crystal at a temperature of 10 K were measured under two-photon and single-photon excitation. The luminescence under two-photon and single-photon excitation revealed a difference in the structure of the spectra.
Авторлар туралы
V. Lukanin
Prokhorov General Physics Institute
Email: karasik@lst.gpi.ru
Ресей, ul. Vavilova 38, Moscow, 119991
A. Karasik
Prokhorov General Physics Institute
Хат алмасуға жауапты Автор.
Email: karasik@lst.gpi.ru
Ресей, ul. Vavilova 38, Moscow, 119991
Қосымша файлдар