Decay of H2O2 under the action of the colloidal catalyst based on iron(III) oxides in a neutral medium


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The catalytic activity of the colloidal catalyst based on iron(III) hydroxide was studied in the decomposition of H2O2 in a neutral medium (pH 6.7). A colloidal micellar solution of iron(III) hydroxide after preparation was kept at 19–20 °С for 2 or 20 h without additives or with C2H5OH additives. The decomposition of H2O2 under the action of the colloidal catalyst (20 h) proceeds via the first-order reaction with the decay rate constant kd = 1.26•10–4 s–1, whereas the decay rate of the first-order reaction is kd = 0.77•10–4 s–1 for the colloidal catalyst (2 h) prepared in the presence of C2H5OH.

Sobre autores

L. Pisarenko

N. N. Semenov Institute of Chemical Physics, Russian Academy of Sciences

Autor responsável pela correspondência
Email: pissarenkolm@mail.ru
Rússia, 4 ul. Kosygina, Moscow, 119991

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Springer Science+Business Media, LLC, part of Springer Nature, 2018