The parameters of atomic interaction pair potential for 13C diamond have been determined from experimental data on the ratio of Raman frequencies for isotopically different diamonds. Based on these parameters, an equation of state and baric dependences of 13C diamond lattice properties at 300 K have been calculated. Specifically, the Debye temperature; the first, second, and third Grüneisen parameters; elastic modulus; thermal expansion coefficient; heat capacity; surface energy; and pressure derivatives of these parameters along a 300 K isotherm have been determined. The results have been compared with available data for diamond having a natural isotopic composition, i.e., for 12.01C.
Об авторах
M. Magomedov
Institute for Geothermal Problems, Dagestan Scientific Center, Russian Academy of Sciences
Автор, ответственный за переписку.
Email: mahmag4@mail.ru
Россия, Makhachkala, 367030
Дополнительные файлы