Composites of the cBN–Si3N4 system reinforced by SiCw for turning tools


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The cBN–Si3N4–SiCw composites with different SiCw contents up to 20 vol % have been produced at high pressure of 8.0 GPa and high temperature of 2500 K. It has been defined that the Young modulus of the composites were within 740–846 GPa, the Vickers hardness and fracture toughness values were 37.5–42.0 GPa and 11.4–12.9 MPa·m1/2, respectively. An important feature of the composite microstructure is the breaking of SiCw as a result of HPHT action. It has been shown that at the addition of 10 vol % SiCw to the structure of a cBN–Si3N4 composite the interrupted turning of hardened steel results in the flank wear reduction up to 20%.

Негізгі сөздер

Авторлар туралы

A. Osipov

Institute of Advanced Manufacturing Technology; Bakul Institute for Superhard Materials

Хат алмасуға жауапты Автор.
Email: Dialab@ism.kiev.ua
Польша, 37a Wroclowska St., Krakow, 30-011; vul. Avtozavods’ka 2, Kiev, 04074

P. Klimczyk

Institute of Advanced Manufacturing Technology

Email: Dialab@ism.kiev.ua
Польша, 37a Wroclowska St., Krakow, 30-011

S. Cygan

Institute of Advanced Manufacturing Technology

Email: Dialab@ism.kiev.ua
Польша, 37a Wroclowska St., Krakow, 30-011

Iu. Melniichuk

Bakul Institute for Superhard Materials

Email: Dialab@ism.kiev.ua
Украина, vul. Avtozavods’ka 2, Kiev, 04074

I. Petrusha

Bakul Institute for Superhard Materials

Email: Dialab@ism.kiev.ua
Украина, vul. Avtozavods’ka 2, Kiev, 04074

L. Jaworska

Institute of Advanced Manufacturing Technology

Email: Dialab@ism.kiev.ua
Польша, 37a Wroclowska St., Krakow, 30-011

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Allerton Press, Inc., 2016