Improving the production of pipe steel


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Melts of pipe steel (strength class K52) obtained at the casting and rolling complex of AO OMK (a branch of AO OMK-Stal’) are analyzed. The initial data correspond to a set of 30 melts. The production system includes batch preparation, steel production in an arc furnace, treatment in a ladle–furnace unit, vacuum treatment (with microalloying and modification), hot rolling, and cutting of the rolled steel into sheet and strip. The basic factors affecting steel quality are identified. The rejection of the steel produced is mainly due to brittle and undeformable nonmetallic silicate inclusions. Changes in the process so as to reduce the content of nonmetallic silicate inclusions are recommended.

Авторлар туралы

A. Lopatenko

Moscow State Institute of Steel and Alloys

Хат алмасуға жауапты Автор.
Email: salat1313@yandex.ru
Ресей, Moscow

D. Orekhov

AO OMK, AO OMK-Stal’

Email: salat1313@yandex.ru
Ресей, Vyksa

A. Semin

Moscow State Institute of Steel and Alloys

Email: salat1313@yandex.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Allerton Press, Inc., 2016