Effect of Mn, Al, Ni, and C Content on the Equilibrium Phase Composition of Alloys Based on the Fe–Mn–Al–Ni–C System


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

A Thermo-Calc program is used to calculate isothermal and polythermal sections of diagrams and phase composition for alloys of the Fe–Mn–Al, Fe–Mn–Al–Ni, and Fe–Mn–Al–Ni–C systems. Phase diagrams are used to study the effect of nickel, aluminum, manganese, and carbon on the equilibrium structure of alloys of the Fe–Mn–Al–Ni–C system. Concentration ranges are determined for existence of single-phase γ-alloys in the range 1000–1200°C. It is established that achievement of a considerable aluminum content (10%) and existence of increased specific strength for austenitic alloys of the Fe–Mn–Al–Ni–C system containing not less than 5% Ni is possible with a manganese content of not less than 20% and carbon not less than 1.4%.

作者简介

L. Kaputkina

National University of Science and Technology MISiS

编辑信件的主要联系方式.
Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

A. Svyazhin

National University of Science and Technology MISiS

Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

D. Kaputkin

National University of Science and Technology MISiS

Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

V. Bazhenov

National University of Science and Technology MISiS

Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

A. Bronz

National University of Science and Technology MISiS

Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

I. Smarygina

National University of Science and Technology MISiS

Email: kaputkina@mail.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media New York, 2016