Corrosion and Physical-Mechanical Properties of Cr–P–W Alloy Obtained by Electrodeposition from Water–Dimethylformamide Electrolytes


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Cr–P–W protective coatings are obtained by electrodeposition from water–dimethylformamide solutions based on chromium(III) chloride, with the addition of sodium phosphinate and sodium tungstate. The resulting alloys contained up to 8 wt % of phosphorus and 1.5 wt % of tungsten, as well as some carbon. The resulting coatings are characterized by satisfactory corrosion resistance in corrosive environments containing chloride ions. The number of through pores in the coatings became negligible with a coating thickness more than 15 μm, providing sufficient protective ability of the developed coatings.

作者简介

A. Telezhkina

Mendeleev University of Chemical Technology

Email: Madjerre@mail.ru
俄罗斯联邦, Moscow, 125047

V. Kuznetsov

Mendeleev University of Chemical Technology; Frumkin Institute of Physical Chemistry and Electrochemistry

编辑信件的主要联系方式.
Email: Vitkuzn1@mail.ru
俄罗斯联邦, Moscow, 125047; Moscow, 119071

E. Filatova

Mendeleev University of Chemical Technology

Email: Madjerre@mail.ru
俄罗斯联邦, Moscow, 125047

N. Nekrasova

Mendeleev University of Chemical Technology

编辑信件的主要联系方式.
Email: Madjerre@mail.ru
俄罗斯联邦, Moscow, 125047

V. Zhulikov

National Research Nuclear University MEPhI

Email: Madjerre@mail.ru
俄罗斯联邦, Moscow, 115409

V. Kolesnikov

Mendeleev University of Chemical Technology

Email: Madjerre@mail.ru
俄罗斯联邦, Moscow, 125047

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2019