The main forms and geometric parameters of chipping during diamond surface grinding are determined on the basis of studying features of the formation Y–TZP-ceramic edge morphology. A correlation is revealed between grinding depth, longitudinal and transverse feed with chipping geometric parameters.
作者简介
V. Kuzin
FGBOU VO Moscow State Technological University Stanki
编辑信件的主要联系方式.
Email: kyzena@post.ru
俄罗斯联邦, Moscow
S. Fedorov
FGBOU VO Moscow State Technological University Stanki
Email: kyzena@post.ru
俄罗斯联邦, Moscow
S. Grigor’ev
FGBOU VO Moscow State Technological University Stanki
Email: kyzena@post.ru
俄罗斯联邦, Moscow
补充文件