Research in the Field of Preparing Molded and Unmolded Refractories Based on High-Alumina HCBS. Part 7. Sintering and Secondary Mullite Formation of Materials Based on Composite Composition HCBS During Nonisothermal Heating and Isothermal Firing1


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The effect of nonisothermal heating in a high-temperature dilatometer and isothermal heating in the range 900 – 1600°C on sintering and secondary mullite formation for specimens based on composite composition HCBS, including with refractory clay additions, is studied. Maximum shrinkage values of 0.4 – 1.3% depending on composition are noted with nonisothermal heating up to 1200 – 1250°C or after isothermal firing at 1100 – 1200°C. Specimen growth index (up to 2.0 – 2.5%) after high-temperature firing depends on SiO2 content that indicates the volume of secondary mullite formed.

Авторлар туралы

Yu. Pivinskii

OOO NVF Kerambet-Ogneupor

Хат алмасуға жауапты Автор.
Email: pivinskiy@mail.ru
Ресей, St. Petersburg

P. Dyakin

FGBOU VPO St. Petersburg State Technological University (Technical University)

Email: pivinskiy@mail.ru
Ресей, St. Petersburg

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media New York, 2017