Research in the Field of Preparing Molded and Unmolded Refractories Based on High-Alumina HCBS. Part 11. Composite Composition HCBS (Fuzed Corundum-Bauxite, Sintered Bauxite, Quartz Glass) and Some Properties of Materials Based Upon Them1


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

HCBS of composite composition are prepared by combined wet grinding using fuzed corundum-bauxite containing 93.4% Al2O3 (45%) and sintered Chinese bauxite (45%) as basic materials. The additional component within the composition of the milling charge is very fine quartz glass (10%). The effect of firing temperature in the range 900 – 1600°C on material sintering and mullitization is studied. Values of ultimate strength in bending of 150 MPa are achieved after firing specimens at 1200°C. The material sintering (shrinkage) and mullitization temperature ranges are established.

Авторлар туралы

Yu. Pivinskii

OOO NVF Kerambet-Ogneupor

Хат алмасуға жауапты Автор.
Email: pivinskiy@mail.ru
Ресей, St. Petersburg

P. Dyakin

FGBOU VPO St. Petersburg State Technological University (Technical University)

Email: pivinskiy@mail.ru
Ресей, St. Petersburg

L. Ostryakov

OAO Dinur

Email: pivinskiy@mail.ru
Ресей, Pervoural’sk

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2017