Varying the Granulometric Composition of an Electrofused-Corundum-Based Ceramic with a Porcelain Binder to Control its Open Porosity and Strength


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

A study is made of a strong porous ceramic based on granular mixes of a filler—electrofused corundum with particle sizes of 2 – 3 and 0.5 mm (95 wt.% of the mix) — and a porcelain binder (5 wt.%). Several mixes were prepared with different values for the 2 – 3 mm/0.5 mm ratio of filler-particle sizes: 0/95, 35/60, 40/55, 45/50, 50/45, and 95/0. The specimens were pressed at pressures of 25, 50 and 100 MPa and fired at temperatures of 1350 and 1450°C. The sintered specimens ranged from 19 to 143 MPa in ultimate flexural strength and 17 to 26% in open porosity. The results are attributed to the formation of a framework in the semifinished product along with regions outside the framework. The new porous permeable ceramic is promising for use in the form of filters and supports for ceramic membranes.

Авторлар туралы

A. Belyakov

Russian University of Chemical Technology

Хат алмасуға жауапты Автор.
Email: av_bel@bk.ru
Ресей, Moscow

Zaw Oo

Russian University of Chemical Technology

Email: av_bel@bk.ru
Ресей, Moscow

N. Popova

Russian University of Chemical Technology

Email: av_bel@bk.ru
Ресей, Moscow

Ye Min

Russian University of Chemical Technology

Email: av_bel@bk.ru
Ресей, Moscow

Kyaw Oo

Russian University of Chemical Technology

Email: av_bel@bk.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media New York, 2016