Strength and Granulometric Composition of Dry-Quenched Blast-Furnace Coke at PAO NLMK
- Autores: Klyukin S.N.1
-
Afiliações:
- PAO Novolipetsk Metallurgicheskii Kombinat (NLMK)
- Edição: Volume 62, Nº 9 (2019)
- Páginas: 408-410
- Seção: Coke
- URL: https://ogarev-online.ru/1068-364X/article/view/226927
- DOI: https://doi.org/10.3103/S1068364X19090035
- ID: 226927
Citar
Resumo
The dependence of the mechanical strength of coke on its granulometric composition is determined for the coke shop at PAO NLMK. The smaller fractions produced from the >80 mm fraction on crushing conform to a normal (Gaussian) distribution. Under the same mechanical load, larger coke pieces are less likely to retain their initial size and more likely to disintegrate. The 40–60 mm class most improves the mechanical strength of blast-furnace coke. With increase in content of this class, the coke will be stronger.
Palavras-chave
Sobre autores
S. Klyukin
PAO Novolipetsk Metallurgicheskii Kombinat (NLMK)
Autor responsável pela correspondência
Email: klyukin_sn@nlmk.com
Rússia, Lipetsk
Arquivos suplementares