MMK Blast Furnace Operation with a High Proportion of Pellets in a Charge. Part 2*
- Autores: Pavlov A.V.1, Onorin O.P.2, Spirin N.A.2, Polinov A.A.1
-
Afiliações:
- Magnitogorsk Metallurgical Combine (MMK)
- Ural Federal University
- Edição: Volume 60, Nº 7-8 (2016)
- Páginas: 653-657
- Seção: Article
- URL: https://ogarev-online.ru/0026-0894/article/view/238937
- DOI: https://doi.org/10.1007/s11015-016-0346-z
- ID: 238937
Citar
Resumo
Results are given for calculation of blast furnace operation with a high proportion of Sokolovo-Sarbaiskii Metallurgical Production Association unfluxed pellets with a different content of local agglomerate. It is shown that with an increase in the proportion of unfluxed pellets (up to 60%) in a loading charge in order to achieve the required blast furnace slag basicity charging limestone into the furnace is necessary. In order to reduce the weight of loaded “raw” limestone, it is necessary to produce agglomerate with high basicity. As the proportion of pellets increases in a loaded charge, there is a reduction in blast furnace slag magnesia content. In order to increase slag magnesium oxide concentration, it is expedient during agglomerate preparation to use a combined basic flux consisting of 70% normal and 30% dolomitized limestone.
Palavras-chave
Sobre autores
A. Pavlov
Magnitogorsk Metallurgical Combine (MMK)
Autor responsável pela correspondência
Email: alexandr.pavlov.v@yandex.ru
Rússia, Magnitogorsk, Chelyabinsk Region
O. Onorin
Ural Federal University
Email: alexandr.pavlov.v@yandex.ru
Rússia, Ekaterinburg
N. Spirin
Ural Federal University
Email: alexandr.pavlov.v@yandex.ru
Rússia, Ekaterinburg
A. Polinov
Magnitogorsk Metallurgical Combine (MMK)
Email: alexandr.pavlov.v@yandex.ru
Rússia, Magnitogorsk, Chelyabinsk Region
Arquivos suplementares