Structure, Mechanical Properties and Fracture Surface Features of Structural Steels Subjected to Deformation-Heat Treatment


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

A comparative study is made of the structure, mechanical properties and crack growth micromechanisms of 09G2S, 25 and 35X steel pipes after different versions of deformation and heat treatment, including cold plastic deformation of highly tempered material by radial forging and subsequent annealing. It is established that the maximum strength of the test steels is achieved after cold radial forging (CRF) with a degree of deformation of 55% and subsequent annealing at 300 °C. It is shown that CRF and annealing at 600 °C leads to formation of an ultra-fine-grained structure as a result of which reliability properties are achieved similar to a highly tempered condition with retention of improved strength properties. Features of the structure are revealed that is formed during CRF. The micromechanism of crack growth after heat and deformation-heat treatment is studied. Analysis is provided for elements of the failure surface after dynamic tests.

Авторлар туралы

G. Shaimanov

Perm’ National Research Polytechnic University

Хат алмасуға жауапты Автор.
Email: shamanD3@gmail.com
Ресей, Perm’

M. Simonov

Perm’ National Research Polytechnic University

Email: shamanD3@gmail.com
Ресей, Perm’

A. Pertsev

Perm’ Scientific Research Technological University

Email: shamanD3@gmail.com
Ресей, Perm’

Yu. Simonov

Perm’ National Research Polytechnic University

Email: shamanD3@gmail.com
Ресей, Perm’

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019