Use of Heterogenization for Improving Alloy AA5083 Superplasticity Indices


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The microstructure and superplasticity indices are compared for specimens of alloy AA5083 prepared by two technologies: using intermediate heterogenization annealing and without it. As a result of heterogenization β -phase is separated that during recrystallization stimulates new grain growth, and therefore the grain size within specimens is smaller by almost a factor of two than for specimens not subjected to annealing. Use of heterogenization annealing provides a relative elongation up to 650% at 550°C and a constant strain rate of 1·10−3 sec−1, and lower residual porosity. Sheet prepared by this technology makes it possible to increase forming rate by several factors.

Авторлар туралы

V. Portnoi

National Research Technology University MISiS

Хат алмасуға жауапты Автор.
Email: portnoy@misis.ru
Ресей, Moscow

O. Yakovtseva

National Research Technology University MISiS

Email: portnoy@misis.ru
Ресей, Moscow

A. Kishchik

National Research Technology University MISiS

Email: portnoy@misis.ru
Ресей, Moscow

A. Kotov

NIU VShÉ, Moscow Institute of Electronics and Mathematics

Email: portnoy@misis.ru
Ресей, Moscow

S. Medvedeva

National Research Technology University MISiS

Email: portnoy@misis.ru
Ресей, Moscow

A. Mikhailovskaya

National Research Technology University MISiS

Email: portnoy@misis.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2018