Magnetic Properties of Hard Magnetic Alloy Fe – 28% Cr – 13.4% Co – 2% Mo – 0.5% Si


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The method of regression analysis is used to obtain equations describing the dependences of magnetic hysteresis properties of magnetically hard powder alloy Fe – 28% Cr – 13.4% Co – 2% Mo – 0.5% Si on regimes of thermomagnetic treatment (the temperatures of the start of the treatment and the rates of cooling in magnetic field). The determined treatment modes make it possible to obtain in an alloy with a coercive force Hc up to 40 kA/m, a residual induction Br up to 1.2 T, and a maximum energy product (BH)max up to 25 kJ/m3. The alloy may find application in the production of rotors of synchronous hysteresis-reluctance motors.

作者简介

T. Vompe

A. A. Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences

编辑信件的主要联系方式.
Email: tvompe@gmail.com
俄罗斯联邦, Moscow

I. Milyaev

A. A. Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences

Email: tvompe@gmail.com
俄罗斯联邦, Moscow

V. Yusupov

A. A. Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences

Email: tvompe@gmail.com
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media New York, 2017